Toner Laser Waterslide Decal paper for Ceramic mug

Toner Laser WaterSlide Decal Paper for Ceramic Mug

      Toner Laser Waterslide Decal Paper printed by digital printing presses, color laser printers, or color laser copy printers with flat feed and flat output, such as  HP Indigo 6K, Ricoh Pro C7500, Xerox® Color 800i/1000i , Canon iR-ADV DX C3935, OKI Data C941dn, ES9542, Konica Minolta AccurioLabel 230, and vinyl cutters or die cutter with Edge positioning combination, for all your Ceramic mug projects.  

laser toner waterslide decal paper for ceramic mug

Toner Laser waterslide decal paper

Product Code: WS-L-150, WS-DL-300, WS-SL-300
Specification:
A4 (210mm X 297mm) – 100 sheets/bag,
A3 (297mm X 420mm) – 100 sheets/bag,
A(8.5”X11”)- 100 sheets/bag,
B(11”X17”) – 100 sheets/bag, 33cm X300M /Roll,other specifications are requirement.
Printers Compatibility: HP Indigo, OKI, Konica-Minolta, Xerox, Canon, Ricoh etc.

Toner Laser WaterSlide Decal Paper for Ceramic Mug


laser toner waterslide decal paper for ceramic mug

White porcelain

Toner Laser Waterslide WS-L-150

laser toner waterslide decal paper for ceramic mug 202

Ceramic mug

Toner Laser Waterslide WS-L-150

laser toner waterslide decal paper for ceramic mug 201

Porcelain bottle

Toner Waterslide paper WS-L-150

Toner Laser WaterSlide Decal Paper for Ceramic Mug

Step 1. Print patterns by Toner Laser printers01

Step 2. Cut patterns by vinyl cutting plotters.2

 Step 3. Submerge you pre-cut decal in 30~55°C (Celsius) water for about 30~60 seconds or until the middle of the decal can easily slide around. Remove from water.WSL-150S

Step 4. Slide the printed side up onto the crafts, and gently scrape away the water droplets and air bubbles between the printed side and the crafts with a damp towel (polyester/nylon blends) or soft rubber scraper4

Step 5. Air dry for 2 hours, or bake at 35°C for 60 minutes. This removes moisture and prevents air bubbles from forming during high-temperature baking. Baking is necessary; bake at 120°C~150°C for 30 minutes. The optimal baking temperature and time should be tested beforehand. After baking, allow to cool naturally to room temperature. Do not attempt to scrape, rub, or pry the finished product, as it needs to be left to dry naturally for at least 24 hours to achieve optimal durability.5

Note: 
1. Towel is made of 88.3% polyester/11.7% nylon fiber blends, brushing

 

Alizarin Technologies Inc.
Add: 901~903, NO.3 building, UNIS SCI-TECH Park, Fuzhou High-Tech Zone, Fujian, China.
Tel: +86-591-83766293/83766295 Fax: +86-591-83766292
Website: https://www.alizarinchina.com/laser-metallic-waterslide-decal-paper-product/ 

Europe
Ms. Wendy
e-mail: marketing@alizarin.com.cn, whatsapp:  https://wa.me/8613506996835
cell phone/wechat: +86 13506996835

Middle East & Africa
Ms. Sunny
e-mail: pro@alizarin.com.cn, whatsapp:  https://wa.me/8613625096387
mobile/wechat: +86 136 2509 6387


Post time: Sep-10-2026

  • Previous:
  • Next:
  • Send your message to us: