Digital Press Konica Minolta AccurioPress C14010S for Printing on Ceramic Cups!

Digital Press Konica-Minolta AccurioPress C14010S for Printing on Ceramic Cups!

    In the spirit of constantly rethinking what’s possible. The new C14010/S and C12010/S series is the successor to the C14000 series, building upon the already ultra-efficient, and super-reliable press to further drive innovation and maximize production. Working alongside the new IQ-601 Intelligent Quality Optimizer to deliver unparalleled color control, consistency, and full color profiling, all at the touch of a button. Additionally, the C14010S and C12010S will mark Konica Minolta’s introduction into 5th color Production Print Cut-Sheet market with White Toner.

   But its direct suitability for ceramic glass cups is limited due to the substrate's properties and the press's ink and printing process. The Pretty-Film developed by our company can easily print on ceramic cup with original toner.
   Pretty-Film (PF-150) that can be printed by Konica-Minolta AccurioPress C14010S/C12010S with flat feed and flat output for all your Ceramic cups/mugs/tea cups. pre-treatment of FJ5 with images to ensure proper ink adhesion, then water slide decals onto un-coated Ceramic cups,  After baking in an electric oven at 130°C~145°C for about 5~10 minutes, After cooling to room temperature, tear off the surface film to get the finished product. The outstanding features of the Pretty-Film are that it does not require pre-coating, and No-Cut. It is also heat-resistant, weather-resistant and washable.

AccurioPress C12010S-2

Product name: PF-150
Product name: Pretty -Film
Main specifications:
A4 (210mm X 297mm) – 100 sheets/pack,
A3 (297mm X 420mm) – 100 sheets/pack,  33cm X 300 meter /roll, 
Laser Printers: Konica-Minolta AccurioPress C14010S / C12010S
Highlight features:  Original toner Only, low temperature baking, No Pre-coating required, No-Cut. Heat-resistant, weather-resistant, and washable.

Digital Press Konica-Minolta Accurio Press C14010S for Printing on Ceramic Cups


AccurioPress C12010S-2

Black Ceramic Mug

AccurioPress C12010S-3

Glass bottle

AccurioPress C12010S-1

Black Ceramic Mug

Step by step from WaterSlide to baking:

step 1. Laser printing:

The printing settings of laser printers of different brands and models are not exactly the same. Please read the operating instructions of the laser printer carefully or consult the laser printer sales agent for laser printing settings.

step 2. Pre-coating:

Soak a sanitary napkin in the Pre-Coat FJ5 pretreatment liquid and gently wipe the laser-printed coating surface. Let it dry naturally for about 5 minutes.
Note: There should be no water droplets. If there are any, wipe them dry with a dry cotton ball.

step 3. Water slide:

Soak in warm water (water temperature is about 30~45 °C) for about 30~60 seconds, until the Pretty-Film (PF-150) can be easily separated from the based paper.

step 4. Remove bubbles

With the printed surface facing down, press the backing paper to separate it from the film, leaving the film on the tiles product. Press the film and gently slide it to a suitable position. Use a rubber melon or a wet towel (88.3% polyester/11.7% nylon fiber blends) to gently scrape the water droplets and bubbles between the film and the tile product.

step 5. baking:

Set the electric baking temperature to 130°C~145°C and the time to 5~8 minutes. The optimal temperature and time can only be determined after multiple tests.
ceramics tile products need to be heated up slowly to the required temperature to avoid sudden temperature changes and spontaneous explosion of the tile.
Put the ceramics tile in the electric oven, close the door, and adjust the time knob to 5~10 minutes. When the baking time is reached, open the oven door, put on high-temperature resistant gloves, take out the ceramics tile, and place the ceramics tile on a heat-resistant table.

step 6. Film tearing:

Let it cool naturally for about 30~60 minutes and start to tear off the film from the corners.

step 7. baking:

Set the electric baking at higher temperature to 170°C~190°C and the time to 5~8 minutes for Better colorfastness 

Precautions:

Please do not try to scrape, rub or pick at the finished product, as it needs to be left for at least 24 hours to achieve the best fastness.

Tiles absorb water very well, so please do not soak them in water to avoid producing a lot of bubbles during baking, which will cause goose bumps in the photos.

For more application scenarios, please visit https://www.alizarinchina.com/pretty-film-3-product/

or contact with:

Asia-Pacific & Australia
Ms. Tiffany
e-mail: sales@alizarin.com.cn WhatsApp:  https://wa.me/8613506998622
mobile/WeChat: +86 135 0699 8622

Europe
Ms. Wendy
e-mail: marketing@alizarin.com.cn  WhatsApp: https://wa.me/8613506996835
mobile/WeChat: +86 135 0699 6835

Fuzhou Alizarin Technologies Inc.
TEL: 0086-591-83766293/83766295, FAX: 0086-591-83766292

WEB: https://www.AlizarinChina.com/
ADD: 901~903, NO.3 building, UNIS SCI-TECH Park, Fuzhou High-Tech Zone, Fujian, China.


Post time: May-03-2026

  • Previous:
  • Next:
  • Send your message to us: